Licensed Professional Engineers |
Search/

Request a free quote

Free tool screening estimate

Reference Electrode Converter and CP Criterion Translator

Converts a structure-to-electrolyte reading between copper/copper sulfate, silver/silver chloride, calomel, hydrogen and zinc electrodes, with the −850 mV criterion on each.

Tool referenceDE-TOOL-10730

Method
Electrode potentials against SHE, UFC 3-570-06 Table 2-1
Electrodes
CSE, Ag/AgCl, SCE, SHE, zinc
Output
Reading and criterion on every electrode

This reference electrode converter restates a cathodic protection reading taken with one electrode on any other. The −850 mV criterion on a saturated copper/copper sulfate electrode is −790 mV on a silver/silver chloride electrode in seawater and −775 mV on a saturated calomel electrode, from the electrode potentials published in UFC 3-570-06 and by the University of Cambridge.

Reference electrode converter and CP criterion translator

Enter a structure-to-electrolyte reading and the electrode it was taken with. The tool restates it on every other common reference electrode, shows the −850 mV copper/copper sulfate criterion on each one, and says how the reading compares with it. The answer updates as you type.

The converter needs JavaScript®. The electrode potentials it uses are in the table on this page.

Quick start Fills in the form. Change anything after.

The reading

The meter reading of the structure against the reference electrode, as recorded. Cathodic protection readings are usually negative (structure negative to the electrode).

The electrode the reading was taken with. Silver/silver chloride electrodes differ with their filling solution: check the label. Zinc values are nominal (±0.1 V in the source).

Type of reading
Temperature (optional)

Result

−850 mV on copper/copper sulfate: at or more negative than −850 mV

−850 mV was taken on a saturated copper/copper sulfate electrode, the electrode the criterion is stated on.

This is an instant-off reading. UFC 3-570-06 (2-1.2.4.2) states the polarized criterion as a polarized potential of at least −850 mV against a saturated copper/copper sulfate electrode.

The 100 mV polarization criterion compares two readings taken with the same stable electrode, so it is 100 mV on any electrode (UFC 3-570-06, 2-1.2.4.3).

On copper/copper sulfate
−850 mV
On Ag/AgCl seawater
−790 mV
−850 mV CSE on your electrode
−850 mV

Converting a reading does not make it a valid criterion check. On readings include voltage drops, and the criteria have conditions and exceptions. See CP readings explained, or ask an engineer.

Potential scale: the zero of each electrode and your readingYour reading −850 mV on Copper/copper sulfate, saturated (CSE) is −850 mV on copper/copper sulfate, at or more negative than −850 mV.−1.0−0.8−0.6−0.4−0.2−0.00.20.4V vs SHE−850 mV CSECSEAg/AgCl swAg/AgCl satSCESHEZnYour reading
Shaded: at or more negative than −850 mV against copper/copper sulfate. Scale in volts against the standard hydrogen electrode.

Your reading and the criterion on every electrode

ElectrodePotential, V vs SHE at 25 °CSourceYour reading−850 mV CSE is
Copper/copper sulfate, saturated (CSE)+0.316UFC 3-570-06, Table 2-1−850 mV−850 mV
Silver/silver chloride, seawater (0.6 M NaCl)+0.256UFC 3-570-06, Table 2-1−790 mV−790 mV
Silver/silver chloride, saturated KCl+0.222UFC 3-570-06, Table 2-1−756 mV−756 mV
Silver/silver chloride, 1 M KCl+0.235DoITPoMS (Cambridge)−769 mV−769 mV
Silver/silver chloride, 0.1 N KCl+0.288UFC 3-570-06, Table 2-1−822 mV−822 mV
Saturated calomel (SCE)+0.241DoITPoMS (Cambridge)−775 mV−775 mV
Standard hydrogen electrode (SHE)0Definition−534 mV−534 mV
Zinc, saline solution (nominal)−0.79 ±0.1UFC 3-570-06, Table 2-1+256 mV ±100+256 mV ±100
Zinc, soil (nominal)−0.80 ±0.1UFC 3-570-06, Table 2-1+266 mV ±100+266 mV ±100
Full results and steps
Your reading−850 mV on Copper/copper sulfate, saturated (CSE)
On copper/copper sulfate−850 mV
−850 mV CSE on your electrode−850 mV on Copper/copper sulfate, saturated (CSE)
  1. Copper/copper sulfate, saturated (CSE): 0.316 V against the standard hydrogen electrode.
  2. Copper/copper sulfate: 0.316 V against the standard hydrogen electrode.
  3. On CSE = reading + (E of your electrode − E of CSE) = −850 + (316 − 316) = −850 mV.

Survey data to review?

Dreiym's licensed Professional Engineers run on, instant-off and native potential surveys, and review existing survey data against the criteria that apply to the structure.

Assumptions and limits

Assumptions: each electrode at its tabulated potential, in good condition and with its proper filling solution; zinc electrodes at their nominal value. Temperature: the tool adds the coefficient of UFC 3-570-06 Table 2-1 to the electrode potential, E(T) = E(25 °C) + c × (T − 25 °C). The table gives no temperature range for the coefficients; have an engineer confirm a corrected value before relying on it.

What this does not check: IR drop, mixed metals, stray current, the location of the electrode, or which criteria apply to your structure.

Screening tool: For education and planning. Not a survey interpretation, and not a substitute for a licensed engineer's or a qualified CP specialist's review.

How the calculation works
  • Each electrode has a potential against the standard hydrogen electrode (SHE).
  • A reading on electrode A, restated on electrode X: reading + E(A) − E(X).
  • The −850 mV criterion is stated against saturated copper/copper sulfate; on electrode X it is −850 mV + E(CSE) − E(X).
  • A zinc electrode carries the ±0.1 V of the source into every converted value.
Sources

Sources: UFC 3-570-06, Operation and Maintenance: Cathodic Protection Systems (US Department of Defense, 15 July 2019), 2-1.2.4 and Table 2-1 (which lists the electrodes of NACE SP0169); DoITPoMS, The Nernst Equation and Pourbaix Diagrams, Other reference electrodes (University of Cambridge, CC BY-NC-SA 4.0).

Cite or share this tool

Dreiym Engineering. Reference electrode converter. Method: electrode potentials from UFC 3-570-06 (2019) Table 2-1 and DoITPoMS. https://www.dreiym.com/reference-electrode-converter/

Instructors and shops are welcome to link to this tool or put its address on a handout. It is free, needs no sign-up and works on a phone.

How to use the converter

Enter the reading as recorded, with its sign, pick the electrode it was taken with and say whether it is an on or an instant-off reading. The table under the result gives the same reading and the −850 mV criterion on every electrode. Tick the temperature box to correct the electrodes that have a published coefficient.

How to convert a reading to another reference electrode

  1. Identify the electrode. For silver/silver chloride, note the filling solution or whether it sits in seawater: each has its own potential.
  2. Record the reading with its sign. Keep the unit (mV or V) and the meter connection the same for every reading.
  3. Look up both electrodes against the hydrogen electrode. Use one consistent table of potentials, such as UFC 3-570-06 Table 2-1.
  4. Add the difference. Reading on the new electrode = reading + potential of the old electrode − potential of the new one.
  5. Compare like with like. Compare a converted reading with the criterion on the same electrode, and an on reading only after the voltage drops have been considered.

Why the same pipe reads differently on different electrodes

A potential is always measured between two things: the structure and the reference electrode. Each electrode has its own fixed potential against the standard hydrogen electrode, the zero of the electrochemical scale, so the same pipe gives a different number on each one. UFC 3-570-06 lists copper/copper sulfate at +0.316 V and silver/silver chloride in seawater at +0.256 V against the hydrogen electrode, so a pipe reads 60 mV less negative on the silver/silver chloride electrode than on copper/copper sulfate.

The criteria on each electrode

ElectrodePotential, V vs SHE at 25 °C−850 mV CSE equalsSource of the potential
Copper/copper sulfate, saturated+0.316−850 mVUFC 3-570-06, Table 2-1
Silver/silver chloride, seawater (0.6 M NaCl)+0.256−790 mVUFC 3-570-06, Table 2-1
Silver/silver chloride, saturated KCl+0.222−756 mVUFC 3-570-06, Table 2-1
Silver/silver chloride, 1 M KCl+0.235−769 mVDoITPoMS, University of Cambridge
Silver/silver chloride, 0.1 N KCl+0.288−822 mVUFC 3-570-06, Table 2-1
Saturated calomel (SCE)+0.241−775 mVDoITPoMS, University of Cambridge
Standard hydrogen electrode (SHE)0−534 mVDefinition
Zinc, saline solution−0.79 ± 0.1+256 mV ± 100UFC 3-570-06, Table 2-1
Zinc, soil−0.80 ± 0.1+266 mV ± 100UFC 3-570-06, Table 2-1

UFC 3-570-06 states the criteria for steel and cast iron piping as at least −850 mV with the protective current applied (the voltage drops other than across the structure-to-electrolyte boundary must be considered), a polarized potential of at least −850 mV, or at least 100 mV of cathodic polarization. The 100 mV criterion compares two readings taken with the same stable electrode, so it is 100 mV whichever electrode is used; UFC adds that it may not be valid where bimetallic corrosion is present, such as a connection to copper grounding.

Temperature

UFC 3-570-06 Table 2-1 gives temperature coefficients of 0.9 mV/°C for copper/copper sulfate, −0.33 mV/°C for silver/silver chloride in seawater, −0.70 mV/°C for saturated KCl and −0.43 mV/°C for 0.1 N KCl. The table also prints 0.5, 0.18 and 0.39 in parentheses, which equal the first three per °F. It gives no coefficient for zinc, and the calomel and 1 M KCl values from Cambridge come without one, so the converter corrects only the four electrodes above. Neither source states a temperature range, so have an engineer confirm a corrected value before relying on it.

Worked examples

  • A dock pile reads −1,050 mV on copper/copper sulfate with the current on. On a silver/silver chloride electrode in seawater the same reading is −990 mV. Both are on readings, so the voltage drop in the water is still in them.
  • A silver/silver chloride electrode in seawater reads −800 mV instant off. On copper/copper sulfate that is −860 mV, at or more negative than the −850 mV criterion.
  • A zinc electrode in soil reads +250 mV. On copper/copper sulfate that is −866 mV, but zinc is nominal to ±0.1 V in the source, so the reading cannot be judged against −850 mV with it.

Why published conversion tables disagree

  • Different values for the same electrode. The 2003 edition of UFC 3-570-06, now cancelled, printed −780 mV on saturated calomel and −800 mV on silver/silver chloride in 25 Ω·cm seawater as equal to −850 mV CSE. The 2019 values give −775 mV and −790 mV.
  • The filling solution. A silver/silver chloride electrode changes with its chloride concentration: UFC lists +0.222 V for saturated KCl and +0.288 V for 0.1 N KCl, 66 mV apart. A table that says only Ag/AgCl leaves that open.
  • Signs and rounding. The Cambridge page gives copper/copper sulfate as −0.318 V against the hydrogen electrode, where UFC gives +0.316 V; the sign differs, and the converter uses the UFC value. Tables printed to 0.1 V, like the zinc rows, round away tens of millivolts.

Common mistakes

  • Dropping the sign, or mixing millivolts and volts.
  • Using a seawater value for an electrode filled with KCl, or the other way round.
  • Comparing an on reading with the polarized criterion without considering the voltage drop.
  • Judging a reading within 100 mV of the criterion with a zinc electrode.

Method and sources

  • UFC 3-570-06, Operation and Maintenance: Cathodic Protection Systems (US Department of Defense, 15 July 2019), 2-1.2.4 (criteria) and Table 2-1, Common Reference Electrodes, which lists the electrodes of NACE SP0169. Approved for public release, distribution unlimited.
  • DoITPoMS, The Nernst Equation and Pourbaix Diagrams, page Other reference electrodes (University of Cambridge): saturated calomel +0.241 V and silver/silver chloride in 1 M KCl +0.235 V at 298 K. Licensed CC BY-NC-SA 4.0; we use the two values with attribution.
  • UFC 3-570-06 (31 January 2003, cancelled), 6-5.1, for the comparison above only.
  • Not used, because we could not read them free: NACE SP0169, AMPP® SP21424 and ASTM® G215. Left out for lack of a free source: silver/silver chloride in 3 M or 3.5 M KCl, and temperature coefficients for calomel and zinc.
  • Method last checked against these sources on 19 November 2026.

Verified against

CasePublished valueThis converter
Ag/AgCl seawater on CSE−0.06 V, UFC 2019 Table 2-1−0.060 V
Ag/AgCl saturated KCl on CSE−0.094 V, same table−0.094 V
Ag/AgCl 0.1 N KCl on CSE−0.028 V, same table−0.028 V
Zinc, soil and saline, on CSE−1.1 V ± 0.1, same table−1.116 V and −1.106 V
Zinc −1.10 V CSE on calomel−0.98 to −1.04 V SCE, UFC 2003 Table 2-2−1.025 V
−850 mV CSE on calomel−780 mV, UFC 2003, 6-5.1−775 mV (different source values)
−850 mV CSE on Ag/AgCl seawater−800 mV in 25 Ω·cm seawater, UFC 2003, 6-5.1−790 mV (2019 value)

These cases are part of the unit tests that run every time the converter is built.

Frequently asked questions

What is −850 mV CSE on a silver/silver chloride electrode?

It depends on the filling solution. With the potentials in UFC 3-570-06 Table 2-1, −850 mV on copper/copper sulfate is −790 mV on silver/silver chloride in seawater, −756 mV with saturated KCl and −822 mV with 0.1 N KCl.

Does the 100 mV polarization criterion change with the reference electrode?

No. It is the difference between two readings taken with the same stable electrode, so the electrode potential cancels out. UFC 3-570-06 notes it may not be valid where bimetallic corrosion is present, such as a connection to copper grounding.

Can a zinc reference electrode be used to check the −850 mV criterion?

UFC 3-570-06 lists zinc at −1.1 V plus or minus 0.1 V against copper/copper sulfate. A reading within about 100 mV of the criterion therefore cannot be judged with zinc; a calibrated copper/copper sulfate or silver/silver chloride electrode can.

Does temperature change a copper/copper sulfate reading?

UFC 3-570-06 Table 2-1 gives a temperature coefficient of 0.9 mV per degree Celsius for the copper/copper sulfate electrode. The converter can apply it, but the table states no temperature range, so a corrected value should be confirmed by an engineer.

When to bring in an engineer

A converted number is the start of a survey review, not the end. Dreiym’s licensed Professional Engineers run cathodic protection potential surveys and interrupted potential surveys. See also how to interpret CP survey data, what an annual CP survey under 49 CFR 192.465 involves, CP testing equipment and the cathodic protection calculator.

Need more than a screening estimate?

We typically respond within one business day.

Request a free quoteor call (866) 621-6920